I have triggered some BGA soldering issues last weeks and got superb responding! We have learnt a lot!. Among answers one warning not using concoat under very large BGAs, could cause pumping effects. Guess Tech-Shot could answer as well, but more gurus at TechNet. Graham N, he must at least have a refresher for me. Got this b4:
1. try skip concoat, best living for BGA solderings
2. if using concoat, always underfill 100% first
3. if using concoat and no underfill first, you'll get closed in gas and contaminations and CTE mismatch >disasters
So, my question is: is 3 above reality for some of you? Don't your balls like such pumping?
Thx in advance
Ingemar Hernefjord
Ericsson Microwave Systems
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|