For what it's worth, I basically agree with you. I have a really good Sonix
ST1000 with a nice collection of transducers.
I have not been extremely successful in getting quality images of the inside
layers of PWBs. As you indicated, the glass mat really messes up the image.
With the proper set-up, one can sometimes pick up gross mousebites, or gross
necking of conductors, but I will not be so bold as to claim the ability to
pick up "cracks" in internal conductors (the boards I've played with are
only 3-4 layers thick).
Suggest the interested parties send samples to Sonix and/or Sonoscan for
evaluation. A contact at Sonix is <[log in to unmask]>
Steve Creswick
CTS RFIM
At 04:55 PM 2/21/01 +0100, you wrote:
>Susan, Hans
>
>If these people are actually talking about an acoustic microscope forget to
use it to find broken traces in a PCB.
>- Cracks in traces tend to be quite thin. The smaller the features you want
to see, the higher the frequencies are you have to use for US- inspection.
On the other hand, the higher the frequencies the smaller the penetration
depth of the ultrasonic waves. If you want a lateral resolution in the 100um
you inspection depth is some um.
>
>- Polymers damp the ultrasound too much. The signal is very weak.
>
>- PCB's are reinforced with glass fibres. Each fibre gives you a signal.
Sure, you can filter that out to a certain extend in the time of flight
graph. However, we tried that and the pictures where not satisfying at all.
It might work for traces right below the soldermask.
>
>
>Maybe one finds some nice pictures for a special case in a prospectus of a
acoustic-microscope vendor but I am not convinced yet that this technique is
applicable for PCB's
>
>Best regards
>
>Guenter
>
>Guenter Grossmann
>Swiss Federal Institute for Materials Testing and Research EMPA
>Centre for Reliability
>8600 Duebendorf
>Switzerland
>
>Phone: xx41 1 823 4279
>Fax : xx41 1823 4054
>mail: [log in to unmask]
>
>---------------------------------------------------------------------------
------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
>Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
>---------------------------------------------------------------------------
------
>
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|