Buried via will be different from PTH because it is typically filled with
resin from the prepreg or some via fill material.

Our finite element results suggest that there might be some increase in the
strain in copper for buried via when filled with resin. This is because
resin has a low elastic modulus (does not help to bear stress) and a high
CTE (help stretch the copper barrel even more). We have observed failures
in buried via, which prompted us to do this FEA study.

Type II, HDI design has buried via from L2 to Ln-1. The reliability of
these vias should be looked into further.

Regards,

Mason

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2