TECHNET Archives

February 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Dennis Fritz <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 26 Feb 2001 23:24:23 EST
Content-Type:
text/plain
Parts/Attachments:
text/plain (46 lines)
In a message dated 2/26/01 7:48:59 PM Eastern Standard Time,
[log in to unmask] writes:

<< is there an underlying Ni diffusion barrier
 between the copper and silver for surface mount applications as there would
 be for Cu/Ni/Au flash? If yes, do you follow the same Ni thickness
 guidelines as for Cu/Ni/Au? If no, why not?

 Is anyone gold wire bonding to an immersion Ag surface for Chip On Board
 applications. I am assuming a Ni barrier layer is used. Correct? >>

Steven -

No, there is no electroless nickel diffusion barrier when using immersion
silver.

Immersion plating is based on the electromotive potential between elements -
that is, the capability to form a "battery". Gold is the most noble element
and could immersion plate on any other metal. Electroless nickel is used as
a barrier because gold immersion plated on copper would form imtermetallic
very rapidly. However, gold can replace nickel from a surface to give
immersion plated gold.

Tin and silver are not as noble as gold, and so far as I know, cannot deposit
over nickel (I am not at my desk as I write). However silver forms
intermetallic very very slowly in contact with copper, and tin forms
intermetallic slowly enough with copper, that you get at least months of
shelf life - depending on immersion plated tin thickness.

Without a nickel barrier, I know of no one wire bonding to silver or tin on
copper. I have no experience with electroplated silver or tin over nickel,
and then wirebonding. However, I be surprised if that is ever done.

Dennis Fritz
MacDermid, Inc

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2