I agree with Kathy, We typically designate no more than three repairs per
assembly, unless it is a special need, (only one left in existence).
but it depends on the complexity of PWB, cost of PWB, and experience of
repair tech that will govern the number.

Tom



>From: Kathy Kuhlow <[log in to unmask]>
>Reply-To: "TechNet E-Mail Forum." <[log in to unmask]>, Kathy Kuhlow
><[log in to unmask]>
>To: [log in to unmask]
>Subject: Re: [TN] Limits to Lifted Pad/Open Trace
>Date: Mon, 26 Feb 2001 09:01:02 -0600
>
>Typically I have used limitations such as no more than 3 pads or traces per
>assembly as long as the pads and traces can be repaired with a high degree
>of assurrance and per the IPC-7721 guidelines. I have seen other
>facilities that use the golden number 5 but with no reasoning behind it.
>
>Kathy
>
> >>> [log in to unmask] 02/26/01 03:04AM >>>
>Hi! I would like to know if there are any standards or norms as to how many
>lifted pads and open traces are allowed for repair within a printed circuit
>board. Does anyone know any guidelines to this? I know IPC says that it
>depends on the customer, well most customer don't know or don't say. Hope
>you guys have more quantitative answers here...
>
>---------------------------------------------------------------------------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt delivery of Technet send the following message: SET
>Technet NOMAIL
>Search previous postings at: www.ipc.org > On-Line Resources & Databases >
>E-mail Archives
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
>additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>---------------------------------------------------------------------------------
><< TEXT.htm >>

_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2