We work with a Philips ESEM and I am quite happy that I don't have to coat my specimen when I look at nonconductive surfaces. In ESEM mode you loose some resolution but working up to 30k wasn't a challenge so far and anyway, whenever I will need high resolution I can still coat my specimen with gold an run the ESEM with high vac.
Regarding the EDX you've got to know what you're interested in. We have a detector with a Be- window. However EMPA also has a WDX for low energy elements. In the beginning we had some problems running the software of the ESEM but now the machine runs perfect.
Have a great day
Guenter
Guenter Grossmann
Swiss Federal Institute for Materials Testing and Research EMPA
Centre for Reliability
8600 Duebendorf
Switzerland
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------