Thank You all for your input!
JF
> -----Original Message-----
> From: Craig Hillman [mailto:[log in to unmask]]
> Sent: Thursday, February 15, 2001 2:33 PM
> To: [log in to unmask]
> Subject: Re: [TN] Burn-in
>
>
> Kathy,
>
> Burn-in is designed to remove latent defects that can lead to infant
> mortality. However, burn-in also takes away some lifetime
> from the products
> and costs time and money. So, there is a benefit and a disadvantage to
> burn-in.
> With a high defect rate in components, burn-in
> provides a large benefit in
> comparison to the disadvantage. This primarily because a low
> stress level is
> necessary to screen out the defects and a large number of defects are
> removed.
> If the defect rate for commercial components is very
> low, the advantages of
> burn-in will not outweigh the disadvantages. The stress level
> necessary to
> screen for defects increases, which can then lead to
> reliabilty problems,
> and very few defects are screened out.
>
> Best Regards,
> Craig
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Kathy Kuhlow
> Sent: Thursday, February 15, 2001 2:09 PM
> To: [log in to unmask]
> Subject: Re: [TN] Burn-in
>
>
> Would that be more when a burn-in cycle takes that components
> to close to
> the maximum threshold? If you degraded a componnet through
> processing then
> the burn-in would verify this.
>
> kathy
>
>
>
> JF,
>
> Due to the increasing reliability of commercial components,
> some studies
> suggest that the stress during burn-in (handling,
> temperature, voltage) will
> not screen out any latent defects but will instead reduce the
> reliability of
> your product.
>
> Best Regards
> Craig
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Bissonnette,
> Jean-Francois
> Sent: Thursday, February 15, 2001 1:14 PM
> To: [log in to unmask]
> Subject: [TN] Burn-in
>
>
> Are burn-in required on every units that come out of
> production or is it
> usually done on
> a sampling basis? If it has to be done on every unit, why is that so?
> We're requested
> to do it on all units, by contract. But some believe that is
> overkill...
> I'm among them.
>
> Any thoughts???
>
> Thanks in advance!
>
> JF
>
>
> WABTEC CORPORATION CONFIDENTIALITY NOTE
> The content contained in this e-mail transmission is legally
> privileged and
> confidential information intended only for the use of the
> individual or
> entity named herein. If the reader of this transmission is
> not the intended
> recipient, you are hereby notified that any dissemination,
> distribution, or
> copying of this transmission is strictly prohibited.
>
> --------------------------------------------------------------
> -------------------
> Technet Mail List provided as a free service by IPC using
> LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with
> following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following
> message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources
> & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm)
> for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> --------------------------------------------------------------
> -------------------
>
WABTEC CORPORATION CONFIDENTIALITY NOTE
The content contained in this e-mail transmission is legally privileged and confidential information intended only for the use of the individual or entity named herein. If the reader of this transmission is not the intended recipient, you are hereby notified that any dissemination, distribution, or copying of this transmission is strictly prohibited.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|