TECHNET Archives

February 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
sean clinton <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 5 Feb 2001 07:28:38 -0600
Content-Type:
multipart/mixed
Parts/Attachments:
text/plain (3186 bytes) , sean.clinton.vcf (313 bytes)
Ed,

Let me begin by stating we use a peroxide/sulfuric acid oxide replacement. We currently use
the Shipley Circubond Oxide Replacement. I like you have found the peel strengths to be lower
than those compared to a conventional oxide. Now with that out of the way, everything else so
far to me has performed better than conventional oxide.
First: the lower peel strengths have never seen any delam between layers. This includes
Neltec, Speedboard, Double treat foil, RTF, G-tek, Hi-Tg, and a few other FR4 like materials.
2: We found controlling copper weight loss to be much easier, thus helping us tighten our
constraints for controlled impedance.
3: All those claims of solder floats and the like have not been wrong yet too!!

We control our conveyorized line by copper etch rate, and line speed. The copper etch rate is
controlled by chemical analysis and automated replenishment. Incidently, we found that on
certain parameters of the pre-clean and pre-dip chemistries, that the chemistry has a much
wider operating window than expected. I contend that controlling the line speed can affect
surface color. Again, I have yet ot see performances decrease due to color variation.

Finally, this system isn't like a conventional oxide, in that it in fact removes copper, and
does not end up weighing more. It actually roughens the copper by microetching. And, it then
passivates the copper with some type of organometallic copper complex. You'd have to read the
patents for more. I hope this helps. ..there is more, but I ramble already.

Regards,

Sean Clinton


Edward Szpruch wrote:

> We are considering replacing of our reduced black oxide and brown oxide
> innerlayer preparation by one of "conveyerised oxide substitions) .
> We made several preliminary tests and the samples were analysed by measuring
> of peel strength.
> The results were considerably lower compared to reduced black oxide
> laminated with epoxy prepreg and brown oxide laminated with polyimide.All
> "oxide substitute" suppliers reacted,that such results are expected,but
> performance of "oxide substitution" should be evaluated taking into account
> tests like solder float,steam test etc.
> I would like to ask PCB manufacturers,how they are controlling the
> properties of their "oxide substitution", especially on
> polyimides,thermount,RCC,teflon etc.
>
> Edward Szpruch
> Eltek , Manager of Process Engineering
> P.O.Box 159 ; 49101 Petah Tikva Israel
> Tel ++972 3 9395050 , Fax ++972 3 9309581
> e-mail [log in to unmask]
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------


ATOM RSS1 RSS2