Dear Technetters,
Can the IWT process be applied to metal parts? We are using tin-lead plating on
some machined pins, but we often face plating problem. Will the IWT process much
expensive than the conventional plating process?

ken

____________________Reply Separator____________________
Subject: Re: [TN] More about white tin (another question)
Author: "TechNet E-Mail Forum." <[log in to unmask]> [log in to unmask]
Date: 2/7/01 4:47 PM

In a message dated 2/7/01 1:34:16 PM, [log in to unmask] writes:

<< What about the concern of tin whisker growth? I believe that, for some

reason, it isn't an issue with the "white" tin process. >>

Immersion White Tin (IWT) is nonporous, and lacks the grain structure
conducive to tin dedritic growth.

IWT is an immersion process, and arguably more of a coating than a plating.
Electro-deposited tin IS NOT recommended as a solderable finish for a variety
of reasons, including a propensity for "whiskers".

For detailed IWT information look to Florida CirTek (Greely, CO), or the
International Tin Research Institute.

--------------------------------------------------------------------------------
-
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet
NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
--------------------------------------------------------------------------------
-

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2