Hallo outhere in th big pcb world
We have a plating problem with PCB ,we plate full electroless nickel
gold ,that means without solder mask.
The problem is,.that from time to time we have stepplating of nickel
This happens only on two types of boards,others boards we plate the same
way and there it never happens stepplating.
We work mith the Ronamerse SMT-Process from Shipley
We have no problems with skip plating in selektiv nickel gold
I hope for good ideas
hopefull greetings from switzerland
Heinz Mader
Ascom AG
CH 3000 Berne
Switzerand
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|