Jowan,
The biggest difference is the hot seal tends to peel
better since it is just a slight melt between the two
plastics. A cold seal is generally a Pressure
Sensitive Adhesive (PSA) and that tends to be more
difficult to peel back for some feeders. However,
most taping machines that you would purchase for lower
volume taping are going to use PSA due to lower cost.
You can check out V-tek online at vtekusa.com for more
info on LV taping machines.
Brad
--- Jowan Iven <[log in to unmask]> wrote:
> Happy New Year to you all,
>
> I'm currently looking for equipment to tape small
> batches of smd's.
> There are two possible systems available 1) "Hot
> seal" and 2) "Cold seal"
> But I can't get a clear picture about all the pro's
> and con's.
>
> I appreciate any input to make a more founded
> decision.
>
>
>
> Jowan Iven
> Process Engineer Manufacturing
> Stork Electronics
>
>
---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC
> using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask]
> with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the
> following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line
> Resources & Databases > E-mail Archives
> Please visit IPC web site
> (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at
> [log in to unmask] or 847-509-9700 ext.5315
>
---------------------------------------------------------------------------------
__________________________________________________
Do You Yahoo!?
Yahoo! Photos - Share your holiday photos online!
http://photos.yahoo.com/
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|