Residual Cu/Sn on the edges could cause step plating. A couple of things
come to mind to solve.
Is your solder strip complete? Can you double pass the part through the
stripper a second time
as a test?
Is your microetch step at mas. Could you remove 80 uins or 2 microns
without imparing the
pads?
I am also aware of another situation where baking at 120 degrees C for one
hour solved the problem.
I don't know a good explanation for this but it maybe worth a test.
Hope this helps.
Marion Graybeal
----- Original Message -----
From: Heinz Mader <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, January 31, 2001 3:16 AM
Subject: [TN] electroless nickel gold stepplating problems
> Hallo outhere in th big pcb world
>
> We have a plating problem with PCB ,we plate full electroless nickel
> gold ,that means without solder mask.
> The problem is,.that from time to time we have stepplating of nickel
> This happens only on two types of boards,others boards we plate the same
> way and there it never happens stepplating.
> We work mith the Ronamerse SMT-Process from Shipley
>
> We have no problems with skip plating in selektiv nickel gold
>
> I hope for good ideas
>
> hopefull greetings from switzerland
>
> Heinz Mader
> Ascom AG
> CH 3000 Berne
> Switzerand
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|