TECHNET Archives

January 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Peter Swanson <[log in to unmask]>
Date:
Wed, 24 Jan 2001 18:41:49 -0000
MIME-Version:
1.0
X-To:
"Marsico, James" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Peter Swanson <[log in to unmask]>
Parts/Attachments:
text/plain (165 lines)
Silver oxides are electrically conductive, one of the reasons why they
are used commonly in electrically conductive adhesives. No, it's the
solder which oxidises and gives rise to problems. In addition, there are
problems with the adhesion of typical Ag epoxies with Sn/Pb solder.

Peter
--
=========================================================
Peter Swanson            [log in to unmask]
INTERTRONICS                http://www.intertronics.co.uk

INTERTRONICS is dedicated to providing quality material,
  consumable and equipment solutions to the electronics
manufacturing and other technology based industries, with
   the highest levels of technical support and customer
                         service.


-----Original Message-----
From: Marsico, James [mailto:[log in to unmask]]
Sent: 24 January 2001 18:28
To: [log in to unmask]
Subject: Re: [TN] silver epoxy & solder coated parts


Hi Glenn,
Thanks for your response.  One more question...  I'm assuming that the
increase in resistance is due to oxidation of the silver at the
epoxy/solder
interface.  If this is true, then why wouldn't oxidation occur with a
Pd/Ag
finish?

Thanks again,
Jim Marsico
EDO Electronic Systems Group
[log in to unmask] <mailto:[log in to unmask]>



        -----Original Message-----
        From:   Pelkey, Glenn [SMTP:[log in to unmask]]
        Sent:   Wednesday, January 24, 2001 12:18 PM
        To:     [log in to unmask]
        Subject:        Re: [TN] silver epoxy & solder coated parts

        Hi Jim,

                We've performed some accelerated tests on this
combination.
Testing
        showed increase in resistance and decrease in adhesion.  Initial
adhesion
        was even poorer than the other combinations.
                Our recommendation was solder terminated components
should
be
        soldered, Pd/Ag terminated should be epoxied.  I've heard others
say
you can
        solder Pd/Ag terminated caps, but the process window is tight
and no
rework
        is allowed.  My opinion is not to do it, not worth the risk.
                As for acceleration, will it last 2 years in your
environment?  I
        don't think so, but I'm just guessing.  Six months, probably.
The
        acceleration model I have would need more data from temperature
and
humidity
        factors.  Don't forget the mechanical shock.

                Have you talked to CALCE?  http://www.calce.umd.edu/

        Glenn

        > -----Original Message-----
        > From: Marsico, James [SMTP:[log in to unmask]]
        > Sent: Tuesday, January 23, 2001 12:35 PM
        > To:   [log in to unmask]
        > Subject:      [TN] silver epoxy & solder coated parts
        >
        > Hello, Technet...
        >
        > Here is an unusual situation.  We have to assemble a surface
mount
        > assembly
        > using silver epoxy.  Some of the components will be solder
coated.
I
        > know,
        > don't bother asking... this is the way it has to be.  The good
thing is
        > that
        > this assembly is a prototype for bench-top laboratory use
only.
There is
        > no
        > harsh environment and needs to operate 1, maybe 2, years.  The
question is
        > does anyone foresee any problems?  What happens when one mixes
toe
two
        > technologies?
        >
        > Thanks,
        > Jim Marsico
        > EDO Electronic Systems Group
        > [log in to unmask] <mailto:[log in to unmask]>
        >


------------------------------------------------------------------------
----
-----
        Technet Mail List provided as a free service by IPC using
LISTSERV
1.8d
        To unsubscribe, send a message to [log in to unmask] with
following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt delivery of Technet send the following
message:
SET Technet NOMAIL
        Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
        Please visit IPC web site (http://www.ipc.org/html/forum.htm)
for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315

------------------------------------------------------------------------
----
-----

------------------------------------------------------------------------
---------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases
> E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
---------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2