Hi JF ( don't know more of your name )
What do you mean with regular tooling. You need some metallographic equipment:
- Moulding equipment to embed the specimen in resin
- Diamond saw, disc or wire.
- Polishing machine with various grinding / polishing disks
. 1 Knuth rotor with paper 180, 250, 400, 1000 or equivalent diamond foils
. 1 disc with diamond 7um
. 1 disc with diamond 3um
. 1 disc with diamond 1um
If you don't have to do micro sections to be done on a regular base they can be polished by hand ( with enough experience of course ) otherwise it is recommendable to use a polishing head that hold your specimen in place applying a constant load.
I believe, if you don't already have a metallographic lab it is the easiest way to let the micro sections to be done.
Have a great day
Guenter
Guenter Grossmann
Swiss Federal Institute for Materials Testing and Research EMPA
Centre for Reliability
8600 Duebendorf
Switzerland
Phone: xx41 1 823 4279
Fax : xx41 1823 4054
mail: [log in to unmask]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|