Hello Everyone,
Perhaps any operators of an anodic protected electroless nickel bath can
help a brother out?
System has been up and running for about 10 months; problems with plate out
onto steel liner in the last 2 months. After passivating and stripping
nickel with nitric acid solution bath and anodic protection works fine for
about 3 operating days, then current flows above 1.5 amps and plate out
ensues (at this point the current increases as the bath temp increases).
I have contacted device manufacturer and the chemistry vendor, but would
appreciate any suggestions from my colleagues.
Thanks in advance,
Russell Burdick
Process Engineer
602-276-1600
_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|