It may be worth asking your customer if they changed the direction of their
vibe to a different plane, ie x vs y vs z. Also, a different way of
applying your loctite could contribute to failures @ heat cycling. Just my
$0.02.
Bill C.
-----Original Message-----
From: Stephen R. Gregory [mailto:[log in to unmask]]
Sent: Monday, January 29, 2001 6:08 PM
To: [log in to unmask]
Subject: [TN] CQFP cracking...
Hi all,
We build a board here that's been built here before, using the same
processes. It is around 8" X 8" polyimide fab, that has two very large
352-pin CQFP's on it. One of the customer requirements is that these parts
be
bonded to the board using Loctite 3615.
So we print paste, then dispense the epoxy, place the parts, and then
cure/reflow the assembly.
With this last build we've done, the customer is reporting that the CQFP's
are cracking during their thermal cycle and vibration tests. This has not
happened before.
Is it possible that we have gotten a suspect batch of parts? Has anybody
else
ever run across this type of problem before?
Thanks!
-Steve Gregory-
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|