George,
my reporting is on more than a hundred pages, I'll cut out some that can be
handled by your server. Your answer will be of great interest. Give me half
a day.
Thx in advance
Ingemar
-----Original Message-----
From: Wenger, George M (George) [mailto:[log in to unmask]]
Sent: den 27 januari 2001 03:04
To: [log in to unmask]
Subject: Re: [TN] Ni/Au solderabilty
Ingemar,
If you forward images to us we'll give you Lucent's "two cents".
Regards,
George
George M. Wenger DMTS
Bell Laboratories Princeton, Supply Network Solutions
Engineering Research Center FMA / AQA / RCA Lab
(609) 639-2769 (Office); 3210 (Lab); 2343 (Fax)
[log in to unmask]
-----Original Message-----
From: Werner Engelmaier [mailto:[log in to unmask]]
Sent: Friday, January 26, 2001 4:22 PM
To: [log in to unmask]
Subject: Re: [TN] Ni/Au solderabilty
Hi Ingemar,
I send an e-mail as soon as you send me the pictures.
Here it is again:
Wow Ingemar,
My favorite 'Katarina' is Ms. Witt of East-German skating fame--now there is
a woman.
Back to SJs. Well I eat my hat--however, not to waffle about it, if this is
really Ni, this solder joint must have been liquid for a loooong
time--certainly not standard reflow. Any abnormal temperature history you
are
aware of?
Whatever it is, to be that brittle and weak to have BGAs fall of the PWBs
reminds me of the industry experience in 1982 when the TI Ag-plated PLCCs
fell of the PCBs at IBM; Ag/Sn IMCs are very weak.
I hope my Qs below may get you thinking in some helpful directions--I
wouldn't expect too much help from the PWB and BGA makers, however.
Q1. How come the Ni plating is recessed below the Cu pad surface rather than
be on top (Photo 1)?
Q2. How sure are you this is really Ni?
Q3. I take it the Ni was Au-plated; where are the Au-IMCs?
Q4. In Photo 2, why is the conclusion: "indicationg unsatisfactory joining
con
ditions?
Q5. In Photo 2, which is the same SJ as Photo 1, it is stated that this pad
is solder mask defined; in Photo 1 there is no indication of the the typical
SMD-solder ball geometry--it sure looks much more like NSMD.
Werner Engelmaier
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|