TECHNET Archives

January 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Kathy Kuhlow <[log in to unmask]>
Date:
Fri, 26 Jan 2001 14:01:35 -0600
Content-Type:
multipart/mixed; boundary="=_431805B7.A0C1AD4C"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Kathy Kuhlow <[log in to unmask]>
Parts/Attachments:
text/plain (643 bytes) , TEXT.htm (1132 bytes)
How would you control an assembly with a fractured solder joint and keep the integrity of the solder joint?  The solder joint could easily continue to degrade and cause field failures.    
Kathy

>>> [log in to unmask] 01/26/01 01:15PM >>>

The IPC standard states that all clipped leads must either be reflowed or checked under 10X magnification. Is this just a standard for single sided boards? If you have a double sided board and a good fillet on the component side of the board and you clipped the leads on the solder side what would be the cause of concern if a joint is fractured on the solder side? 
 
[log in to unmask] 



<!DOCTYPE HTML PUBLIC "-//W3C//DTD HTML 4.0 Transitional//EN"> <HTML><HEAD> <META content="text/html; charset=iso-8859-1" http-equiv=Content-Type> <META content="MSHTML 5.00.2614.3500" name=GENERATOR></HEAD> <BODY style="FONT: 8pt Arial; MARGIN-LEFT: 2px; MARGIN-TOP: 2px"> <DIV>How would you control an assembly&nbsp;with a&nbsp;fractured solder joint and keep the integrity of the solder joint?&nbsp; The solder joint&nbsp;could easily continue to degrade and cause field failures.&nbsp; &nbsp; </DIV> <DIV>Kathy</DIV> <DIV><BR>&gt;&gt;&gt; [log in to unmask] 01/26/01 01:15PM &gt;&gt;&gt;<BR></DIV> <DIV><FONT size=2>The IPC standard states that all clipped leads must either be reflowed or checked under 10X magnification. Is this just a standard for single sided boards? If you have a double sided board and a good fillet on the component side of the board and you clipped the leads on the solder side what would be the cause of concern if a joint is fractured on the solder side? </FONT></DIV> <DIV><FONT size=2></FONT>&nbsp;</DIV> <DIV><FONT size=2><A href="mailto:[log in to unmask]">[log in to unmask]</A> </FONT></DIV></BODY></HTML>