Our chip carrier product is experiencing a very interesting problem.
Random
features on the product are not plating in the Ni cell. A thick Cu seed
layer
with a photo mask is pattern plated in Cu and then goes directly to our
Ni/Au
operation. After Ni/Au we find that some features are totally devoid of
Ni! The
Au still plated (to full thickness) so I know the seed was still intact
(commoned).
The Cu plated well, so I discounted the possibility of a resist residue.
A colleague
mentioned skip plating. I've heard the term before, but I can't find
detailed
information in any of my reference books. Anybody want to fill me in? Or
speculate
on this intriguing phenomenon?
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|