CTE Numbers that I use are typically: X-axis 14ppm/C (from ambient to Tg)
Y-axis 13ppm/C (from ambient to Tg)
Note Tg for FR 404 is 150C and FR 406 is 170C
Bill C.
NorLux Corp.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Mark Gilbert
Sent: Thursday, January 25, 2001 3:19 PM
To: [log in to unmask]
Subject: [TN] TCE for FR-4
Does anyone know the thermal coefficient of expansion for FR-4 offhand?
Best Regards,
Mark Gilbert, Product Engineer
FOX Electronics
For Frequency Control Solutions. . . Fast:
1-888-GET2FOX, ext. 2289
Direct Line: 941-690-2289
Fax: 941-693-1554
http://www.foxonline.com/
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|