TECHNET Archives

January 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 15 Jan 2001 10:14:01 +0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=US-ASCII
From:
Ken Fong <[log in to unmask]>
Parts/Attachments:
text/plain (25 lines)
Thanks for your reply. The pin material is copper.

We do not want to dip solder it immediately because the vendor does not have the
setup and skilled worker to do so. Are there simpler and cheaper process?

____________________Reply Separator____________________
Subject:    Re: [TN] Prevent oxidation
Author: <[log in to unmask]>
Date:       1/13/01 1:27 PM

Better give us the compositions of the pins before we give you a solution.
Copper?

Can you immediately solder dip them after trim?

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2