I would not expect underfill temperatures to cause outgassing.
We have seen excessive preheat cause the underfill to wick aroung the
component leaving a void.
Guy Ramsey
American Competitiveness Institute
Senior Lab Technician / Instructor
610 362-1200 ext 107
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Hann Pang
Sent: Tuesday, December 05, 2000 12:27 PM
To: [log in to unmask]
Subject: [TN] Query: industry standard for pretreating PWB/PCB before
underfilling?
Hi
Can someone help me with the question?? Thank you very much.
I'm posting the above question as a technical marketer for 3M. We're
currently working on underfills and the question is posed in consideration
of the outgassing of the PCBs.
If there is'nt a standard, then the next question is; typically, what are
the pretreating conditions if there is any pretreating at all?
Thanks and regards,
Hann Pang
Technical Markerter
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|