TECHNET Archives

December 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Ingemar Hernefjord (EMW)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 13 Dec 2000 16:04:14 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (89 lines)
Speaking of caps, as far as I can see, then I have the right cause to hang
on. MOS or MIM or MIS, that's wonderful small creatures, not bigger than a
fly's .... Have had some delicate trouble on my desk. From GOhms to kOhms
and lower and no one understand what happened. ESD, supply spikes,wire
bonding..or what? This one: gold/nickel on spin-on glass over doped silicon
and finally backside gold. We found (etched away gold and SEMed or
FIBed)numeral bubbles in the dielectric (spin-on glass)and just wonder if
someone in this forum ever had similar problem and what was the insight? Pf
was 25 and max voltage 100VDC with sudden increase in leakage at 250VDC.
Nearest guy I could find was Ron Anderson at IBM/Fishkill, but there may be
others to speak with?
Just happened to listen
Ingemar Hernefjord
Ericsson Microwave Systems

-----Original Message-----
From: Guenter Grossmann [mailto:[log in to unmask]]
Sent: den 13 december 2000 10:44
To: [log in to unmask]
Subject: [TN] Antw: [TN] Failure analysis of cap: Type analysis and any
lab that cando the job in San Jose Bay Area


Ken

I have seen several causes for leakage in chip capacitors:

Material:

- Choice of the dielectric. Some ceramic materials degrade over time
releasing free ions entrapped in the matrix or change their structure ( NPO-
type ). Some ceramics such as titanate can have semiconductor
characteristics.
- Spacing . Capacitors with high capacitance have more electrodes and
thinner dielectrics which makes leakage more likely than in capacitors with
low capacitance.
To see this you can make microsections, analysis of the material,
measurement of the dielectric resistance, characterisation of the resistance
( or capacitance )- temperature behaviour.


Damage:

Cracks ( don't have to be visible outside ) in the dielectric either by
mechanical stress or thermal stress ( soldering ) are a path where filaments
can grow. Voids in the ceramic matrix have the same effect.
We had the best success by applying a controlled current to the capacitor
while we watched for local heating with an IR- microscope. Once the heated
point was localised we where able to show the failure with a microsection.

Another important analysis tool is some luck. However I try never to rely on
that.

Have a great day

Guenter

Guenter Grossmann
Swiss Federal Institute for Materials Testing and Research EMPA
Centre for Reliability
8600 Duebendorf
Switzerland

Phone: xx41 1 823 4279
Fax :      xx41 1823 4054
mail:     [log in to unmask]

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2