Hi Mark,
We used Double Treat in my last shop and saw the same scratches. The
troubling thing was opening a new pack from the manufacturer and seeing the
scratches. The answer I got back - the scratches were probably cosmetic
but use your judgment. If it was a huge problem wouldn't you see
delamination or have trouble with photoresist adhesion during an in-process
step were it was scratched?
Hans
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Process Engineer
Toppan Electronics, Inc.
770 Miramar Road
San Diego, CA 92126
(858) 695 - 2222 ext. 241
(858) 695 - 6823 fax
[log in to unmask]
-----Original Message-----
From: Mark Hargreaves [mailto:[log in to unmask]]
Sent: Monday, December 11, 2000 1:34 PM
To: [log in to unmask]
Subject: [TN] Scratched double treat material
Hi All,
The double treat inner layer material we use often arrives with surface
scratches - deep enough to be seen, but not deep enough to affect the
underlying copper. These scratches are visible on the finished boards. Is
this a cosmetic defect, or worse? Is board performance affected? Should
our vendor be slipsheeting this material? Which essential question have I
forgotten to ask?
Thanks in Advance,
Mark Hargreaves
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|