TECHNET Archives

December 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"Wenger, George M (George)" <[log in to unmask]>
Date:
Thu, 21 Dec 2000 16:52:45 -0500
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Wenger, George M (George)" <[log in to unmask]>
Parts/Attachments:
text/plain (148 lines)
Lisa,
I'm not sure what ink is on our boards but I'll see if I can find out.  Most
of our boards have nomenclature ink on solder mask.  I'll check to see if I
can find any that has ink on copper.  I think your assumption is correct
that the microetch or chemical bond might be attacking the adhesion.

Regards,

George
George M. Wenger DMTS
Bell Laboratories Princeton, Supply Network Solutions
Engineering Research Center FMA / AQA / RCA Lab
(609) 639-2769 (Office); 3210 (Lab); 2343 (Fax)
[log in to unmask]


-----Original Message-----
From: Lisa Angle [mailto:[log in to unmask]]
Sent: Thursday, December 21, 2000 4:43 PM
To: [log in to unmask]
Subject: Re: [TN] Nomenclature with Immersion Tin/Silver


George,
Are you putting nomenclature directly on bare copper?  We have no problems
with nomenclature on soldermask, its when we put the nomneclature directly
on copper and then put it through an immersion process.  I think we might
be experiencing one of two things, (1) undercut from micro etch and
replacement mechanism or (2) chemical bond attack between the copper and
nomenclature surfaces.  What are your thoughts?  What nomenclature ink are
you using?
Lisa




"Wenger, George M (George)" <[log in to unmask]>@IPC.ORG> on 12/21/2000
04:13:38 PM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to "Wenger, George M (George)" <[log in to unmask]>

Sent by:  TechNet <[log in to unmask]>


To:   [log in to unmask]
cc:

Subject:  Re: [TN] Nomenclature with Immersion Tin/Silver


Lisa,
Most of our boards are SMOBC and many have nomenclature ink applied before
the final surface finish is applied.  To the best of my knowledge, our
board
vendors haven't had problems processing boards with nomenclature ink
through
IAg, OSP, or HASL.

Regards,

George
George M. Wenger DMTS
Bell Laboratories Princeton, Supply Network Solutions
Engineering Research Center FMA / AQA / RCA Lab
(609) 639-2769 (Office); 3210 (Lab); 2343 (Fax)
[log in to unmask]


-----Original Message-----
From: Lisa Angle [mailto:[log in to unmask]]
Sent: Thursday, December 21, 2000 3:46 PM
To: [log in to unmask]
Subject: [TN] Nomenclature with Immersion Tin/Silver


All,
I was wondering how you go about putting nomenclature on copper surfaces
and subsequently processing thru immersion tin or immersion silver without
experiencing nomenclature peel?  I have of course thought of the
alternative which is to process the boards thru immersion processes and
subsequently nomenclature them, however, our current inks require a long
cure time and very high temperature which artificially ages the finishes.
Thanks.
Lisa Angle
Alternative Surface Finish Engineer
Teradyne

----------------------------------------------------------------------------

-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------

-----

----------------------------------------------------------------------------
-----

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2