TECHNET Archives

December 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TOE /Torben Østeraa <[log in to unmask]>
Date:
Mon, 18 Dec 2000 12:07:31 +0100
Reply-To:
Roland Jaquet <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
8bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Roland Jaquet <[log in to unmask]>
Parts/Attachments:
text/plain (72 lines)
Hello Torben,

There is a specialist for plating serving all Europe in Switzerland called
Hoftetter - Markus Hofstetter - They do have capability for up to 1'200 sq
meters per day, and have horizontal and vertical capabilities with the
latest technology.

Markus Hofstetter
Hansruedi Fisher
T +41-41-850-5050
They also have a web site but I do not have the address yet...

Must be with .com or .ch


Very Best Regards

Roland

PCB Consultant - Company Viability - Technical Viability - Technology
Choice - Yield Improvement - Company Strategy - Equipment Choice - Company
Acquisition
Tel. +41-22-880-0405 - GSM (cellphone) +41-79-203-3723 - Fax +41-22-880-0409
Http://www.PCBspecialist.com
21 Grand-Voiret - CH-1228 Plan-Les-Ouates - Geneva - Switzerland
----- Message d'origine -----
De : "TOE /Torben Østeraa" <[log in to unmask]>
À : <[log in to unmask]>
Envoyé : lundi, 18. décembre 2000 10:06
Objet : [TN] pth plating repair


Dear TechNetters,

Does anyone know OF a source for selective electroplating
on individual pth's. I remember to have heard about systems that
would circulating plating solution through the holes while applying
current.?
Could be a service provider,  or could be a supplier of suitable
equipment.

regards

Torben Østeraa
Printca AS


----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2