OK guys. This looks like a really cool system. I'm interested in possibly
using something like this to remove moisture from PWBs prior to being
installed in the oil tank of a high voltage system. Any suggestions on how
long a circuit board should be stored in this cabinet prior to sinking in
oil?
Thanks in advance,
Phil Nutting
Manufacturing Engineer
Kaiser Systems, Inc.
-----Original Message-----
From: Brad L. Matthies [mailto:[log in to unmask]]
Sent: Tuesday, December 05, 2000 5:42 PM
To: [log in to unmask]
Subject: Re: [TN] Dry Nitrogen Storage Cabinets
I concure. We have one of these units in our facility and they are well
worth the investment.
bbarr wrote:
> As an alternative to nitrogen cabinets, you may want to consider a McDry
> desiccant cabinet. Mine keeps the internal RH at 4% without heat or
> nitrogen. They are distributed by Seika Machinery in Torrence, CA.,
> 310-540-7310, www.seikausa.com.
> Many sizes are available.
>
> Bob
>
> Robert Barr
> Manufacturing Engineering
> Formation, Inc.
> Voice: 856-234-5020 x3035
> Fax: 856-234-6679
> email: [log in to unmask]
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of John Maxwell
> Sent: Tuesday, December 05, 2000 9:21 AM
> To: [log in to unmask]
> Subject: [TN] Dry Nitrogen Storage Cabinets
>
> I saw a while back listings of dry nitrogen storage cabinets, stored it on
> one of my computers and now I am away from that one for some time and need
> that information. Could some kind soul please e-mail off line who some of
> the manufacturers were.
>
> Thanks,
>
> John Maxwell
>
>
----------------------------------------------------------------------------
> -----
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
>
----------------------------------------------------------------------------
> -----
>
>
----------------------------------------------------------------------------
-----
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
>
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|