Ruby,
Be aware that most reliability predictions do not take into account failures
at the solder interconnects. Depending upon your parts and your environment,
these failure modes might be your primary reliability concern, not
die-related issues.
Craig
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Ruby Hazen
Sent: Thursday, December 14, 2000 5:57 PM
To: [log in to unmask]
Subject: [TN] Component Category
Hello all:
I'm doing some reliability prediction of electronics equipment. I want to
have some information about the category of the components, such as what's
the differences between IC and semiconductor, what's the differences among
logic IC, analog IC, and digital IC, etc.
In addition, given a part number, how could I know which category it is? For
example, intel firmware hub 82802AB.
Totally no idea. Any information are very welcome.
Thanks, Ruby
____________________________________________________________________________
_________
Get more from the Web. FREE MSN Explorer download : http://explorer.msn.com
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|