You might try to protect them in the wave with a masking pallet. We do quite
a few of those to solve that very problem. You can give me a buzz, Chuck
Smith @ GSC 972-494-1911.
----- Original Message -----
From: Jim Kittel <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, December 14, 2000 2:28 PM
Subject: [TN] Solder Failure During SMT/Wave Solder
> Hi,
> I am encountering solder failures I have never seen before on some type II
> SMT assemblies. These are about 8 x 16 inch mixed technology boards with
> misc SMT parts including some 0.020 inch pitch QFP's and some thru hole
> connectors. The cards are 0.062 and about 8 layers of 1 ounce copper.
> Paste is 63/37 eutectic.
>
> We paste, populate the primary side with SMT, reflow solder, clean,
inspect,
> and then send the board to wave solder area. In wave solder they install
> the thru hole connectors on the primary side and then wave solder. From
> what I know this is an industry standard process.
>
> The problem is that on two QFP's (always the same) the leads can be easily
> lifted right out of the solder fillet after wave solder. (Board has
> cooled.) Sometimes the solder stays on the lead, sometimes it stays on the
> pad. Solder is always fine before wave solder. We attached thermocouples
> to leads on these QFP's and ran the boards back thru the wave solder.
Found
> a lead that peaked below melt temperature and another lead peaked above
> solder melt. The leads between these are the ones that can be easily
pulled
> out of the solder after cooling. In some cases the solder appears dull
and
> grainy, but in other cases it still looks shiny.
>
> Is it possible the solder in these connections is reaching the plastic
> stage, crystallizing and then loosing it's strength? If so, why doesn't
> this happen to others in the industry running this process? We have to
run
> about 3 feet/minute to solder the thru hole connectors to the 1 ounce
> planes. Is the remedy to go even slower to reflow all the top
connections?
> Ran EDX on the solder in the failed connections and saw nothing unusual.
> Any help would be appreciated. I am stumped.
>
> Thanks,
>
> Jim Kittel
> L-3 Communications
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|