Hi Mike - we do limited solderability testing on incoming materials.
Product - commercial and military avionics in a high mix, low volume type
of manufacturing environment. Solderability testing done per JSTD-002A.
Dave Hillman
Rockwell Collins
[log in to unmask]
Mike Sewell <[log in to unmask]>@IPC.ORG> on 12/14/2000 09:09:23 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to [log in to unmask]
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Solderability Testing
If I may, I'd like a quick poll of those of you who do solderability
testing
on incoming material. Please also give your manufacturing enviroment -
volume, mix, commercial or aerospace.
Regards,
Mike Sewell
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------