Jol,
I believe fluoborate baths will tend to leach nickel from stainless steel
anode baskets. I've used graphite baskets with success in bright acid
sulfate tin plating. (If the tin-lead is only used as an etching resist,
you'd do well look at tin plate in your process instead IMO.
George Carroll
[log in to unmask] <mailto:[log in to unmask]>
-----Original Message-----
From: Sprowles, Jol [mailto:[log in to unmask]]
Sent: Tuesday, December 05, 2000 2:00 PM
To: [log in to unmask]
Subject: [TN] Solder Baskets
For plating tin/lead from fluoroborate baths, what is the current wisdom of
using stainless steel baskets for anode balls? Relative strong points of
graphite vs. stainless steel?
Thank you,
Jol Sprowles, Ph.D.
Senior Process Engineer
Tyco / Electronics / Printed Circuit Group - Stafford Division
Phone: (860)684-5881 ext. 263
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|