Patti,
Be very careful! If you use this technique over bare copper, it will
dewet like hell, due to abrasive particles being implanted into the
metal.
Brian
"Goldman, Patricia J." wrote:
>
> Technet colleagues,
>
> My boss came across the term "micro sand blasting" in an article in the
> April 2000 edition of SMT Magazine.
>
> He asked me what that was and of course I did not have an answer. Can
> someone give me a nice description of this operation or process?
>
> The article had to do with Conformal Coatings and the pertinent sentence
> was: "Rework on acrylics and urethanes can be handled using mechanical
> abrasion or micro sand blasting."
>
> Thanks for your help,
> Patty
> Patricia J. Goldman
> PPG Industries, Inc.
> 724-274-3417
> [log in to unmask]
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|