Thanks
Kenny McKee
<kmckee@MJSDE To: [log in to unmask]
SIGNS.COM> cc:
Sent by: Subject: Re: [TN] PCB Corrosion
TechNet
<[log in to unmask]
ORG>
21/11/00
09:50
Please
respond to
"TechNet
E-Mail
Forum.";
Please
respond to
Kenny McKee
Conformal coating will provide protection from the outside conditions. This
coating is put on the board after the assembly process.
Kenneth McKee
PCB Designer
MJS Designs, Inc.
4130 E. Wood Street
Suite 100
Phoenix, Arizona 85040
(602) 437-5068
(602) 437-5299 FAX
mailto:[log in to unmask]
-----Original Message-----
From: Dean Hunt [mailto:[log in to unmask]]
Sent: Monday, November 20, 2000 1:16 PM
To: [log in to unmask]
Subject: [TN] PCB Corrosion
Is anyone having problems with PCB corrosion. We have a number of products
which are showing signs of corrosion on the copper tracks and planes. The
products concerned are in non-air conditioned environment and varying
humidity situations. Does anyone know of a suitable method to protect PCBs
from external elements. I am keen to hear of any known solutions to this
problem.
Thanks
Dean Hunt
CAD Solutions Manager
----------------------------------------------------------------------------
---
Invensys Energy Systems (NZ) Limited, 39 Princess St, PO Box 11-188
Christchurch 8030, New Zealand
Phone: (++64) 3 343-3314, Fax: (++64) 3 348-5100
Phone: (++64) 3 343-7471,DDI
Email: [log in to unmask]
Website: http://www.invensys-energy.co.nz
----------------------------------------------------------------------------
----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|