Hi,
There are two possibilities:
1. Heat shock comming into the wave and comming out of the wave,
this is due to cold air turbulances at the exit point and cold boards
at the entry point. -You need to control the ambient temp. of the boards
prior and after the wave.
2. static electricity and or layout design issues vs. heat transffer.
--
Best Regards,