TECHNET Archives

November 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Furrow, Robert Gordon (Bob)" <[log in to unmask]>
Date:
Mon, 6 Nov 2000 10:53:15 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Ronald Yanuszewski <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Ronald Yanuszewski <[log in to unmask]>
Parts/Attachments:
text/plain (117 lines)
Bob:

Did you do any testing to the bare such as simulated aging or to the
assembled boards such as temperature/humidity cycling, SMD pull testing,
etc.

Ron

----- Original Message -----
From: Furrow, Robert Gordon (Bob) <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, November 06, 2000 10:19 AM
Subject: Re: [TN] IMMERSION SILVER SURFACE FINISH


> Jim,
>
> We have utilized immersion silver as a PWB surface finish on a large
> quantity of boards for the past few years. Our experience has been
excellent
> and it is now the preferred finish at some of our manufacturing locations.
> George Wenger of our research center and I submitted a paper which he
> presented that detailed our qualification and experience (up to that
point)
> at the September 1999 IPC Surface Finish Forum. Since then we have
qualified
> several PWB shops for this use and have qualified another chemistry
vendor's
> process. We have found if stored properly, the finish retains excellent
> solderability for over a year. It handles multiple thermal excursions well
> and has superior hole fill characteristics compared to OSP's. We did see a
> few start-up issues with our initial board vendor, but since then things
> have gone smoothly. To date, I have seen two  relatively minor assembly
> issues. The first is that the surface will darken if exposed to sulfur.
The
> solderability remains good, but cosmetically it was very noticeable. This
> became evident at one location when after the first side surface mount
> operation, boards were placed onto an ESD mat that had a high sulfur
> content. Switching to a new type of mat resolved this issue. The second
> issue is pin contact at ICT. If you are not wave soldering or if you
> selectively wave solder, then some of the test pins may contact silver
> coated pads. If your test fixtures are set up to handle OSP coated boards
I
> would expect no issues, but if they have only tested to solder previously,
> there might be a need to either change probe types or optimize the
fixture.
> As far as cost is concerned I would expect it to be between the cost of an
> OSP coated board and that of a HASL finish. If you would like further
> information please contact me.
>
> Thanks,
> Robert Furrow
> SMT Process Engineer
> Lucent Technologies
> 978-960-3224    [log in to unmask]
>
> > -----Original Message-----
> > From: Jim McMurry [SMTP:[log in to unmask]]
> > Sent: Monday, November 06, 2000 9:05 AM
> > To:   [log in to unmask]
> > Subject:      [TN] IMMERSION SILVER SURFACE FINISH
> >
> > Jim McMurry@PATAPSCO
> > 11/06/2000 09:05 AM
> >
> > I am interested in hereing from anyone who may be using or may have used
> > immersion silver finish on production or prototype pcb's.  I would like
to
> > know
> > the good and bad sides of this finish.  If there are any information
> > resources
> > available on the subject.  Are there any cost comparisons?
> >
> > Thank you all for your time and response.
> >
>
> --------------------------------------------------------------------------
> > -------
> > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> > To unsubscribe, send a message to [log in to unmask] with following text
in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > Search previous postings at: www.ipc.org > On-Line Resources & Databases
>
> > E-mail Archives
> > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> > additional
> > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> > ext.5315
>
> --------------------------------------------------------------------------
> > -------
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2