TECHNET Archives

November 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 13 Nov 2000 15:09:28 EST
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
George Milad <[log in to unmask]>
Parts/Attachments:
text/plain (20 lines)
Immersion Silver is limited by the nature of the reaction.  Immersion implies
that the substrate is the source of electrons needed for reduction of silver
in solution to silver metal.  This ocurrs at the expense of the substrate
metal giving up electrons and going into solution.
20 to 25 uins are acheivable if the reaction was allowed to go on for an
extended time.  The thickness of 170 - 180 uins will require a deposition
method other than Immersion.
George Milad
Shipley Co.
(516)868-8800  X  269

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2