Hi!!
I have heard some PCB manufacturerss capable of delivering 100 microns
FR4 in a multilayer substrate but I don`t know their source for the
prepreg. If you are looking for FR4 without fibre reinforcement,
it would be too brittle (like SR) and may not be useful as a substrate/
board.
regards.
SRINIVASAMURTHY. S
> -----Original Message-----
> From: <Your Full Name> [SMTP:[log in to unmask]]
> Sent: Wednesday, November 01, 2000 1:23 PM
> To: [log in to unmask]
> Subject: [TN] Thin FR#4 substrate
>
> Hi:
> Is there anyone using very thin(thickness) FR#4 substrate instead of
> flex
> cicruit ? It may be kind of FR#4 without fibre glass enforcement. Any
> information are welcome.
>
> regards,
>
> Chan SL
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|