Carol: Thanks, but in accordance with suggested best practice, my
email system here is set to reject any unsolicited file attachment
that big.
More importantly, I believe the IPC server strips out file attachments
anyway to minimise virus problems. It certainly does on the TechNet
forum. What people do there is post the files to an open website place
and people can down load or view them there. [Handy for looking at
"picture problems".]
Mike Fenner
T: +44 1295 722992
F: +44 1295 720937
Visit: www.lasercuttingco.com
----- Original Message -----
From: "Carol Handwerker" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, November 03, 2000 4:51 PM
Subject: [LF] Sn-Ag-Cu phase diagram and eutectic composition
> I have appended two preprints from Journal of Electronic Packaging
for your
> information. The first is a NIST paper describing our experimental
and
> theoretical work on establishing the ternary eutectic in the
Sn-Ag-Cu
> system. The ternary eutectic composition is Sn - 3.5Ag (+-0.3) -
0.9Cu
> (+-0.2) with a eutectic temperature of 217.2deg C (+/-0.2 deg C)
>
> The second paper is on a similar analysis on the Sn-Bi-Pb system.
> If you have questions regarding these, please contact Ursular
Kattner of
> NIST at [log in to unmask]
>
>
----------------------------------------------------------------------
----------
> **************************************
> Carol A. Handwerker
> Chief, Metallurgy Division
> NIST
> 100 Bureau Drive Stop 8550
> Gaithersburg MD 20899-8550
> Office:(301) 975-6158
> Fax:(301) 975-4553
> e-mail:[log in to unmask]
---------------------------------------------------------------------------------
Leadfee Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|