Jim
There is no such thing like a stress / strain curve of Sn63 because of its creep behaviour. What I can offer you is:
- Stress / strain rate curve with the temperature as parameter
- Constitutive equation Strain rate = f ( Stress, Temperature )
Both ( for Sn62Pb36Ag2) you find in the proceedings of the 1997 IEMT Symposium, IEEE Catalogue Number 97CH36068
Title: Lifetime Assessment of Solder Joints on the Base of the Metallurgical Behaviour of Sn62Pb36Ag2
Have a great day
Guenter
Guenter Grossmann
Swiss Federal Institute for Materials Testing and Research EMPA
Centre for Reliability
8600 Duebendorf
Switzerland
Phone: xx41 1 823 4279
Fax : xx41 1823 4054
mail: [log in to unmask]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|