Arturo,
Are you doing a double sided board?  If so would it be due to the screen printer?  Pick and place force on the cap is with in range?  Have you sampled any parts right out of the reel?  

Just some thought.
Brian Holt 
[log in to unmask]
SMT Supervisor


-----Original Message-----
From:   Arturo Urias [SMTP:[log in to unmask]]
Sent:   Thursday, November 02, 2000 12:21 PM
To:     [log in to unmask]
Subject:        [TN] Cracked capacitors question

Dear subscribers:

I have seen in a few of our products some cracked capacitors. The cracks
are very small and it is usually very difficult to see them, even under a
high maginification microscope. When we reflow one side of the capacitor
with the solder iron, the capacitor completely separates. In a few cases I
have seen the cracks even before we touch it up with the solder iron, so I
know that somehow it is happening before touchup. This problem has been
experienced on boards that do not go through the wave. There are other
components like resistors and even other capacitors that do not show the
same problem, even on the same product. The capacitors are 805s.

Any ideas as to what is causing this?

Thanks!

Arturo Urias
National Instruments

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2