Trevor,
What is it shorting to?? Is it across the R/C or is it shorting to etch?
DT
At 12:08 PM 11/1/00 -0500, you wrote:
> Has anyone ever seen solder shorts under an smt resistor that has been
>glued on a board and then wave soldered?
> The boards go through the standard surface mount process of screen printing
>the glue, placement of components and curing the glue. Then the boards
>receive solder reflow for the top side of the board, on to hand assembly and
>then wave solder. During all in process inspection even after wave solder,
>the boards look good. When the boards get to test it is a different story.
>Randomly across the bottom side of the board, the side that was wave
>soldered, we will get short conditions on various caps and resistors. If you
>look at the component nothing appears to be wrong, but when the component is
>removed you can see solder on the under side of the component and on the
>pcb.
> This problem has just cropped up, so I find it a complete mystery.
>
>Thanks in advance.
>
>
>Trevor Goddard,
>SMT Supervisor
>XLTEK
>(905) 829-5300 x 348
>[log in to unmask] <mailto:[log in to unmask]>
>
>---------------------------------------------------------------------------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>Search previous postings at: www.ipc.org > On-Line Resources & Databases >
>E-mail Archives
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|