Ceramic caps can be problematic for several reasons:
* Make sure that the caps are not adjacent to "breakaway"
areas, or edges of boards that are cut apart. We've recently
worked a problem where V-scrored boards were then
sheared using a double pizza cutter arrangement, and the
caps still cracked.
* Make sure that they are not mounted near connectors
requiring high tension to remove or install. The flex in
the panel when doing such, is enough in many cases
to break the cap. Likewise, ensure that the test process
or any other handling operation does not flex the board.
* Verify your placement equipment to ensure that
it's traveling the correct amount in the Z axis and
not trying to push the cap through the board. :-)
I believe Kemet has a great treatise on using
ceramic caps, for free if you ask for it!
Let us know how it works out!
John
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|