In a message dated 11/02/2000 1:24:11 PM Central Standard Time,
[log in to unmask] writes:
> Dear subscribers:
>
> I have seen in a few of our products some cracked capacitors. The cracks
> are very small and it is usually very difficult to see them, even under a
> high maginification microscope.
Another possible problem is the board being flexed too much after reflow.
Here's a couple of links that talk about that problem:
http://www.paktron.com/techarticles/tech399/b3-99.htmlhttp://www.syfer.com/ta_02.htm
-Steve Gregory-
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------