Kenco is out of business. The Omegameter 500 is manufactured by Alpha Metals
/ Cookson Electronics. Their website is:
http://www.scscookson.com/instruments/
I do not know if they still support the Omegameter 500, but you may want to
give them a call. Their number is (770) 619-5250.
Good Luck.
Lee Whiteman
Senior Manufacturing Engineer
ACI / EMPF
Telephone: (610) 362-1200; Ext. 208
FAX: (610) 362-1290
E-Mail: [log in to unmask] <mailto:[log in to unmask]>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Stuart Korringa
> Sent: Thursday, November 02, 2000 10:42 AM
> To: [log in to unmask]
> Subject: [TN] Omegameter 500 help needed
>
>
> We have an Omegameter 500 that we need to use. The last operator
> is retired and
> the user's manual is missing since we moved to a new building.
> Searching the web
> under the manufacturer, Kenco Industries, drew a blank, at least
> the way I set
> up the search engines.
>
> Can someone on the TechNet guide us to how to set up and use the machine?
>
> Thanks,
>
> Stu Korringa
> Smiths Industries
> Grand Rapids, Michigan
> [log in to unmask]
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> Search previous postings at: www.ipc.org > On-Line Resources &
> Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|