TECHNET Archives

November 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Shirley Xiao <[log in to unmask]>
Date:
Wed, 29 Nov 2000 03:20:04 -0800
Content-Type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Shirley Xiao <[log in to unmask]>
Parts/Attachments:
text/plain (33 lines)
  My friend pass me another question. I hope someone
can give some inputs.
  The application is a mobile phone keypad (gold
plated), Motorola's engineer insists that it is not
acceptable if we can see the patten of glass fabric.
The microsection shows there is no weave exposure or
weave texture(use 0.014" H/H laminate,construction is
2 ply of 7628)
  1. Is it true that the circuit board surface is more
rough if we use 7628?
  2. What can do to improve the surface quality? Use
2116 instead of 7628 or modify the resin content of
7628 prepreg?
  3. Is there any related specification?

  Thanks in advance!
  Shirley


__________________________________________________
Do You Yahoo!?
Yahoo! Shopping - Thousands of Stores. Millions of Products.
http://shopping.yahoo.com/

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2