I've seen it also, but not from wave solder. It usually happens when you
print paste and then glue. When you reflow the paste and cure glue at the
same time, you get solder paste trapped in the glue, causing a short. Check
some parts right after reflow, you may find your problem. An xray can help
here.
-----Original Message-----
From: Trevor Goddard [mailto:[log in to unmask]]
Sent: Wednesday, November 01, 2000 12:08 PM
To: [log in to unmask]
Subject: [TN] solder under chip components
Has anyone ever seen solder shorts under an smt resistor that has been
glued on a board and then wave soldered?
The boards go through the standard surface mount process of screen printing
the glue, placement of components and curing the glue. Then the boards
receive solder reflow for the top side of the board, on to hand assembly and
then wave solder. During all in process inspection even after wave solder,
the boards look good. When the boards get to test it is a different story.
Randomly across the bottom side of the board, the side that was wave
soldered, we will get short conditions on various caps and resistors. If you
look at the component nothing appears to be wrong, but when the component is
removed you can see solder on the under side of the component and on the
pcb.
This problem has just cropped up, so I find it a complete mystery.
Thanks in advance.
Trevor Goddard,
SMT Supervisor
XLTEK
(905) 829-5300 x 348
[log in to unmask] <mailto:[log in to unmask]>
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|