James, at the Kemet plant in Fountain Inn, SC, I visited several years ago, layers of metallized green tape we cofired.  They had a clean room (class ???) and used filtered water to make the slurry.  It was fascinating.  Lou Hart

----------
From:   James W. High[SMTP:[log in to unmask]]
Sent:   Tuesday, October 03, 2000 1:35 PM
To:     [log in to unmask]
Subject:        [TN] multilayer chip capacitors

Hello everybody!

Will someone please save me some time?  Are multilayer ceramic chip
capacitors made from multiple layers of "green tape" and cofired, or are
they printed onto individual ceramic substrates and then assembled somehow?
 Any links to the details of fabrication will be appreciated.

Thanks,
James W. High

_________________________________________________________________________
HIGH, JAMES W.                             E-mail  [log in to unmask]

Mail Stop 390                            Systems Engineering Competency
1 East Durand Street            Electronic Applications Technology Branch
NASA Langley Research Center                      Building 1238, Room 155
Hampton, VA 23681-2199                                (tel)  757-864-5416
                                                      (fax)  757-864-8092

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2