Hans,
Depending on the width of the scratches it is probably cosmetic only. The treatment
scratches easily. The scratches may add to adhesion. Complain to the unnamed party
anyway, it is poor workmanship at the least.
Chuck Brummer
Acuson (soon to be something else)
Hinners Hans Civ WRALC/LYPME wrote:
> Hi All,
>
> We've gotten a shipment of Double Treated laminate (I won't mention names)
> with slight scratches and scuff marks on every panel (front and back).
> The treatment is gone and copper is showing through in some areas.
>
> Is this normal?
> Do we have to worry about delamination after pressing up?
>
> Hans
>
> ~~~~~~~~~~~~~~~~~~~
> Hans M. Hinners
> Materials Engineer (Process & Manufacturing)
> Warner Robins Air Logistics Center
> Avionics Production Division
> Precision Attack/ Radar/Manufacturing Branch
> Engineering Section
> 380 Second Street, Suite 104
> Building: 640, Mail Stop: LYPME
> Robins AFB, GA 31098-1638
> Voice: (478) 926 - 1970 Fax: (478) 926 - 7164
> mailto:[log in to unmask]
> http://www.robins.af.mil
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|