TECHNET Archives

October 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"d. terstegge" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 27 Oct 2000 09:05:27 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (50 lines)
Hi Brett,

Right now we're trying to get rid of baking by putting all our bare boards in a dry storage room. But in unconditioned storage, in a wet climate (we're in the Netherlands), baking the boards is advised by most bare board vendors, especially for polyimide !  Don't know about G-200.

Kind regards,

Daan Terstegge
Unclassified mail
Personal Website: http://www.smtinfo.net


>>> <[log in to unmask]> 10/26 12:52 pm >>>
Fellow Technetters,

     particularly those of you who assemble.  Recently we had
some boards made of Isola(allied signal) G-200(BT-Epoxy) exhibit
delam during wave solder.  These boards were made in week 19-00,
wrapped in paper and shelved until week 34-00 when they were
assembled.  The assembler says nobody bakes boards anymore.
My understanding is that G-200 and Poyimide are extremely hydrscopic,
more so than standard epoxies, and lab test show that the defective area
was high in water content.  If this had been the case back in week 19-00
when I leveled them, they would have delamed then.
   Do you assemblers still bake prior?  Should these materials be baked prior
to assembly ?  How should they be stored and handled ?  Steve are you there ?

Thanks Guys

Brett Austin
Nationwide Circuits Inc
[log in to unmask] 

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives