Hey Jim Terveen... you know we have a laser marker... didn't you used to
use it? How are you? By the way, can't laser one particular part because
it's Kovar (iron based) and can rust if nickel is penetrated.
Thanks,
Jim M.
-----Original Message-----
From: Terveen, James @ NARDAEAST
[SMTP:[log in to unmask]]
Sent: Wednesday, October 18, 2000 3:40 PM
To: [log in to unmask]
Subject: Re: [TN] INK MARKING
In a past life we used to use a laser marking machine to mark nickel
plated
heatsinks on circuit boards. Maybe you might have a laser marker in
your
facility that you can use to mark the parts. Because if I remember
the
marking always seemed to come off the nickel heatsinks during
cleaning.
-----Original Message-----
From: Marsico, James [mailto:[log in to unmask]]
Sent: Wednesday, October 18, 2000 3:23 PM
To: [log in to unmask]
Subject: [TN] INK MARKING
Having trouble ink marking (epoxy ink) on nickel plated housings.
Marking
comes off during in-line aqueous cleaning process. Any suggestions?
Thanks,
Jim M.
----------------------------------------------------------------------------
-----
TechNet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
TechNet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|